Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.172 - 0.241 GPa | 25.0 - 35.0 ksi | Dry |
Unifrax Foamfrax® Isofoam® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |
|||
Modulus of Rupture | 0.172 - 0.241 GPa | 25.0 - 35.0 ksi | Dry |
Unifrax Foamfrax® RG Plus Insulation Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process.. |