Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.138 - 0.207 GPa @Treatment Temp. 982 °C, Time 86400 sec |
20.0 - 30.0 ksi @Treatment Temp. 1800 °F, Time 24.0 hour |
Fired |
Unifrax Foamfrax® Isofoam® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |