Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0214 GPa | 3.10 ksi | |
Pyrotek RFM Light density refractory composite material The RFM material is a composite made of fiberglass fabric and a wollastonite slurry. It can be shaped to very complex and thin parts. It has a very good behavior against molten aluminum alloys.App.. |
|||
Modulus of Rupture | 0.0214 GPa | 3.10 ksi | |
Pyrotek RFM™ Autopour Ladle Light density refractory composite material ApplicationsHigh pressure die casting Gravity die casting Sand casting AdvantagesLight weight No pre-heating required Low thermal heat sink Excellent mechanical properties Excellent resistance to er.. |