Polymer Property : Modulus of Rupture = 3.00 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0172 - 0.0207 GPa
2.49 - 3.00 ksi
Pyrotek AFB-2300 HT Structural Board
AFB-2300 HT is a ceramic fiber board which features a unique alumina-based binder. This white board is heat-treated to eliminate all possible out-gassing and withstands temperatures up to 1260°C.H..