Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00830 GPa | 1.20 ksi | At Use Limit; ASTM C268 |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |
|||
Modulus of Rupture | 0.00830 GPa @Temperature 1260 °C |
1.20 ksi @Temperature 2300 °F |
ASTM C268 |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |
|||
Modulus of Rupture | 0.00830 - 0.0103 GPa | 1.20 - 1.49 ksi | ASTM C133 |
Ceradyne Thermo-Sil® Castable 120 Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |