Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.007848 - 0.00981 GPa @Temperature 1400 °C |
1.138 - 1.42 ksi @Temperature 2550 °F |
|
Chosun Refractories CRAG-L44 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |