Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00700 GPa | 1.02 ksi | |
Pyrotek Pyrite N-14 Refractory Board Pyrotek N-14 is a fiberglass reinforced calcium silicate board specifically developed for the non-ferrous industry. The superior strength and unique formulation of Pyrotek N-14 makes it the preferr.. |