Mechanical Properties Metric English Comments
Modulus of Rupture 0.00500 GPa
0.725 ksi
parallel to thickness
Zircar Refractory Composites RS-99-60 Refractory Sheet
ZRCI Refractory Sheet Type RS-99-60 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani..