Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00400 GPa | 0.580 ksi | EN 993-6: 1995 |
Skamol Group Moler M-EXTRA 'E' Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |