Polymer Property : Modulus of Rupture = 0.225 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00155 GPa
0.225 ksi
dry
Imerys KT Castâ„¢ Kaolin
KT Cast is a coarse-grained, white firing kaolin that is used primarily in casting bodies based on its fast casting and exceptional deflocculation characteristics.Information provided by Imerys