Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.200 GPa @Temperature 1400 °C |
29.0 ksi @Temperature 2550 °F |
Hot |
Sharadaa Ceramics Sharada RFC-95 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |