Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00115 GPa | 0.167 ksi | As Received, Parallel to thickness |
Zircar Ceramics ECO-27B Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer.. |