Polymer Property : Modulus of Rupture = 0.119 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000820 GPa

@Temperature 1260 °C,
Time 86400 sec
0.119 ksi

@Temperature 2300 °F,
Time 24.0 hour
Parallel to Thickness
Zircar Ceramics ECO-27A Alumina-Silica Insulation
This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer..
Modulus of Rupture 0.000820 GPa

@Temperature 1260 °C,
Time 86400 sec
0.119 ksi

@Temperature 2300 °F,
Time 24.0 hour
Parallel to Thickness
Zircar Ceramics ECO-27B Alumina-Silica Insulation
This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer..