Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.000138 - 0.000345 GPa | 0.0200 - 0.0500 ksi | Dry |
Unifrax Fiberfrax® Vari-Form™ A Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |