Polymer Property : Modulus of Rupture = 0.0386 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0386 GPa

@Temperature 816 °C
5.60 ksi

@Temperature 1500 °F
Hot
Pyrotek Pyrocast AL3 Abrasion & Alkali Resistant Refractory Castable
Pyrocast AL3 is suited for use in aluminum melting equipment and metal transfer areas where sever wear or alkali attack are a factor. Pyrocast AL3 is a high-purity mullite based refractory with low..