Modulus of Rupture 0.0345 GPa

@Temperature 704 °C,
Time 360000 sec
5.00 ksi

@Temperature 1300 °F,
Time 100 hour
AK Steel 441 Ferritic Stainless steel
AK Steel 441 is a 17-18% by weight, chromium and columbium bearing ferritic stainless steel which provides good high-temperature strength (exceeding that of Types 409 and AK Steel 439 LT Stainless S..