Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0180 GPa | 2.61 ksi | parallel to thickness |
Zircar Refractory Composites RS-99W Refractory Sheet Type RS-99W boards can be moistened with water and molded into any desired shape. After low temperature bake-out of 300°C (570°F) boards are unaffected by moisture.Information provided by ZIRCAR R.. |
|||
Modulus of Rupture | 0.0180 GPa | 2.61 ksi | parallel to thickness |
Zircar Refractory Composites ZIRCAL-95 Refractory Board Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for.. |