Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00520 GPa | 0.754 ksi | |
Zircar Ceramics HASH-60 Alumina-Silica Insulation ZIRCAR Ceramics Alumina-Silica Insulation Type HASH-60 is a hardened insulation board used primarily for its high temperature dielectric strength in high power electrical switching equipment. Inform.. |