Modulus of Rupture 0.00448 GPa
0.650 ksi
Dry Modulus of Rupture for 50% clay/50% flint, cast bars
Old Hickory 44-B Kentucky Ball Clay
The 44-B clay is similar to 54-S and is a recommended selection where additional plasticity and strength are important. It is particularly recommended in extruded and plastic processed ceramic formu..