Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00355 GPa | 0.515 ksi | Dry Modulus of Rupture, 50% clay/50% flint, cast bars |
Old Hickory TI-21 Tennessee Ball Clay TI-21 is a very low carbon content clay specifically designed for plastic forming methods. It has excellent oxidation qualities particularly for dense volume stoneware or vitreous ceramic pieces. Th.. |