Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00300 GPa | 0.435 ksi | |
Pyrotek Pyrocast FSC-2000 Stabilized fused silica cement Pyrocast FSC-2000 eliminates the need for cement pre-mixing or rolling while providing the same outstanding characteristics of all dense fused silica products.ApplicationsAdhesive Coating Patching c.. |
|||
Modulus of Rupture | 0.00300 GPa | 0.435 ksi | EN 993-6: 1995 |
Skamol Group SKAMOLEX V-1100 (800) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |