Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00200 GPa | 0.290 ksi | EN 993-6: 1995 |
Skamol Group SKAMOLEX V-1100 (700) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Modulus of Rupture | 0.00200 GPa | 0.290 ksi | EN 993-6: 1995 |
Skamol Group SKAMOLEX V-1100 (700) Panel Design SKAMOLEX panel designs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and versatil.. |