Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00180 GPa | 0.261 ksi | EN 993-6: 1995 |
Skamol Group Moler LR-1750 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Modulus of Rupture | 0.00180 GPa | 0.261 ksi | EN 993-6: 1995 |
Skamol Group Moler SUPRA Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Modulus of Rupture | 0.00180 GPa | 0.261 ksi | EN 993-6: 1995 |
Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |