Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.000896 - 0.00145 GPa | 0.130 - 0.210 ksi | Dry |
Unifrax Fiberfrax® Vari-Form™ B Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |