Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.000689 GPa | 0.100 ksi | Fired |
Unifrax Fibermax® Duraboard® 17R Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |