Mechanical Properties Metric English Comments
Compressive Modulus 63.4 GPa

@Temperature 121 °C
9200 ksi

@Temperature 250 °F
Dry, 365° Oven Cured; SACMA 1R-94
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Compressive Modulus 63.4 GPa

@Temperature 232 °C
9200 ksi

@Temperature 450 °F
Dry; ASTM D6641
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..