Compressive Modulus 67.6 GPa

@Temperature 71.1 °C
9800 ksi

@Temperature 160 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..