Compressive Modulus 28.1 GPa

@Temperature 232 °C
4080 ksi

@Temperature 450 °F
Hexcel® HexPly® F650 Bismaleimide Resin with Fiberglass 7781 fabric reinforcement
Laminate Physicals: 53% Fiber volume, 29% Resin content, 0.5% VoidsInformation provided by HexCel
Compressive Modulus 28.1 GPa

@Temperature 24.0 °C
4080 ksi

@Temperature 75.2 °F
Dry
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel