Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
ASTM D695 Modified |
Saint-Gobain Meldin® 2001 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Compressive Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
ASTM D695 Modified |
Saint-Gobain Meldin® 2021 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |