Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 22.8 GPa @Temperature 23.9 °C |
3300 ksi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Compressive Modulus | 22.8 GPa @Temperature 21.1 °C |
3300 ksi @Temperature 70.0 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 22.8 GPa @Temperature -53.9 °C |
3300 ksi @Temperature -65.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 22.8 GPa @Temperature 23.9 °C |
3300 ksi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |