Polymer Property : Compressive Modulus = 1.91 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.0132 GPa

@Strain 20 %
1.91 ksi

@Strain 20 %
ISO-7743
Vicone High Performance Rubber VicoFluorâ„¢ 57FK-GR High Performance Fluoroelastomer Rubber
Meets ASTM D2000 fluoroelastomer 75 Durometer.