Polymer Property : Compressive Modulus = 1.13 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.00780 GPa

@Strain 25 %
1.13 ksi

@Strain 25 %
ISO-7743
Vicone High Performance Rubber VicoFluorâ„¢ 06FK-BR High Performance Fluoroelastomer Rubber
Meets ASTM D2000 fluoroelastomer 60 Durometer.