Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00190 GPa @Strain 10 % |
0.276 ksi @Strain 10 % |
ISO-7743 |
Vicone High Performance Rubber VicoSil™ 139DLK-BL High Performance Silicone Rubber FDA Approved |
|||
Compressive Modulus | 0.00190 GPa @Strain 25 % |
0.276 ksi @Strain 25 % |
ISO-7743 |
Vicone High Performance Rubber VicoSil™ 139DLK-CL High Performance Silicone Rubber FDA Approved |