Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00158 GPa @Strain 25.0 % |
0.229 ksi @Strain 25.0 % |
|
Vicone High Performance Rubber VicoFluorâ„¢ C105LF-BL High Performance Fluoroelastomer Information provided by Vicone |