Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00126 GPa @Strain 10.0 % |
0.183 ksi @Strain 10.0 % |
|
Vicone High Performance Rubber VicoSilâ„¢ C306E-GR High Performance Silicone Rubber Information provided by Vicone |