Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00840 GPa @Strain 20 % |
1.22 ksi @Strain 20 % |
ISO-7743 |
Vicone High Performance Rubber VicoSealâ„¢ 07EK-BK High Performance EPDM Rubber Peroxide Cured |