Compressive Modulus 0.00180 GPa

@Strain 5 %
0.261 ksi

@Strain 5 %
ISO-7743
Vicone High Performance Rubber VicoSil™ 139DLK-BL High Performance Silicone Rubber
FDA Approved
Compressive Modulus 0.00180 GPa

@Strain 20 %
0.261 ksi

@Strain 20 %
ISO-7743
Vicone High Performance Rubber VicoSil™ 139DLK-CL High Performance Silicone Rubber
FDA Approved