Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00170 GPa @Strain 10 % |
0.247 ksi @Strain 10 % |
ISO-7743 |
Vicone High Performance Rubber VicoSilâ„¢ 139DLK-CL High Performance Silicone Rubber FDA Approved |