Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00160 GPa @Strain 5 % |
0.232 ksi @Strain 5 % |
ISO-7743 |
Vicone High Performance Rubber VicoSilâ„¢ 139DLK-CL High Performance Silicone Rubber FDA Approved |