Mechanical Properties Metric English Comments
Compressive Modulus 0.00131 GPa

@Strain 20.0 %
0.190 ksi

@Strain 20.0 %
Vicone High Performance Rubber VicoSil™ 0591EK-CL High Performance Silicone Rubber
Information provided by Vicone
Compressive Modulus 0.00131 GPa

@Strain 20.0 %
0.190 ksi

@Strain 20.0 %
Vicone High Performance Rubber VicoSil™ C240Q-RD High Performance Silicone Rubber
Information provided by Vicone