Mechanical Properties Metric English Comments
Compressive Strength 93.2 MPa

@Temperature 1100 °C
13500 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC45 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 93.2 MPa

@Temperature 1100 °C
13500 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC60 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 93.2 MPa

@Temperature 1100 °C
13500 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC70 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 93.2 MPa

@Temperature 110 °C
13500 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Compressive Strength 93.2 MPa

@Temperature 110 °C
13500 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics ZAP 010 Smart Cast Application
Special Properties: High Strength CastableIndustry: Non-FerrousApplication: Aluminum Melting/Holding FurnaceInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 93.2 MPa

@Strain 10.0 %
13500 psi

@Strain 10.0 %
ASTM D695
Daelim H&L Plavis-G40 DF 40% Graphite Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is..
Compressive Strength 93.2 MPa

@Temperature 1350 °C,
Time 10800 sec
13500 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories BLC Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 93.2 MPa

@Temperature 1500 °C,
Time 10800 sec
13500 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CTL-VBC Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 93.2 MPa

@Temperature 1000 °C,
Time 10800 sec
13500 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 93.2 MPa

@Temperature 110 °C,
Time 86400 sec
13500 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories SFC-90SC High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 93.2 MPa

@Temperature 1350 °C,
Time 10800 sec
13500 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SFC-UL90S High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).