Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 8.64 MPa @Strain 0.200 %, Temperature 23.0 °C |
1250 psi @Strain 0.200 %, Temperature 73.4 °F |
ASTM D695 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Compressive Strength | 8.64 MPa @Strain 0.200 %, Temperature 23.0 °C |
1250 psi @Strain 0.200 %, Temperature 73.4 °F |
ASTM D695 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |