Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 427 MPa @Temperature 21.1 °C |
62000 psi @Temperature 70.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 427 MPa @Temperature 23.9 °C |
62000 psi @Temperature 75.0 °F |
Dry; Autoclave, 50 psi, 90min; ASTM D695 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |