Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 421 MPa @Temperature 82.2 °C |
61000 psi @Temperature 180 °F |
Dry; Vacuum/Oven Cured; SACMA 1-94 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Compressive Strength | 421 MPa @Temperature 23.9 °C |
61000 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s.. |