Polymer Property : Compressive Strength = 5950 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 41.0 MPa

@Strain 2 %
5950 psi

@Strain 2 %
ISO 604
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data)
Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro..