Compressive Strength 0.400 - 0.600 MPa

@Temperature 100 °C
58.0 - 87.0 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable
Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning ..