Polymer Property : Compressive Strength = 54000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 372 MPa

@Temperature 23.9 °C
54000 psi

@Temperature 75.0 °F
Wet; ASTM D695
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:..
Compressive Strength 372 MPa

@Temperature 149 °C
54000 psi

@Temperature 300 °F
Wet; ASTM D695
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..