Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1.00 - 5.00 MPa

@Temperature 1260 °C
145 - 725 psi

@Temperature 2300 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable
Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va..