Polymer Property : Compressive Strength = 49300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 340 MPa

@Temperature 23.0 °C
49300 psi

@Temperature 73.4 °F
Elisto THERMOSTAR® 4000 Mold Insulation Material
Insulation of clamping platesInformation provided by elisto
Compressive Strength 340 MPa

@Temperature 23.0 °C
49300 psi

@Temperature 73.4 °F
Elisto THERMOSTAR® LC 6000 Insulation Material
Pattern material. Insulation materials for mechanical engineering.Information provided by elisto