Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 31.4 MPa @Temperature 110 °C, Time 86400 sec |
4550 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CTL ASP-N Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |